The alloy series, what the temper codes mean, and typical strength and fabrication ratings for 1100, 2024, 3003, 5052, 5083, 6061, 6063, 7075 and cast tooling plate.
STEP · STL · IGES · DWG · DXF · SLDPRT · and more
No CAD file? Describe your project instead
Aluminum alloys are named by a four-digit number whose first digit gives the main alloying element, followed by a temper code that says how the metal was strengthened. Together they set strength, how well the part machines, bends, welds and anodizes, and what it costs. For most custom parts the choice comes down to 5052-H32 for bent sheet, 6061-T6 for machined and general structural parts, and 7075-T6 when 6061 is not strong enough. The tables below cover those and the other alloys that show up on drawings.
Wrought aluminum alloy series
Heat-treatable alloys gain strength from solution heat treatment and aging (T tempers). Non-heat-treatable alloys gain it only from cold work (H tempers).
| Series | Main alloying element | Heat treatable | Character | Common alloys |
|---|---|---|---|---|
| 1xxx | None (99.00% aluminum min) | No | Soft, very formable, highest conductivity and corrosion resistance, low strength | 1100, 1050 |
| 2xxx | Copper | Yes | High strength and fatigue resistance, poorer corrosion resistance, generally not arc welded | 2024, 2011 |
| 3xxx | Manganese | No | Moderate strength, very formable, good corrosion resistance | 3003, 3105 |
| 4xxx | Silicon | Mostly no | Lower melting point; mainly welding filler and brazing alloys | 4043, 4047 |
| 5xxx | Magnesium | No | Good strength for a non-heat-treatable alloy, excellent weldability and seawater resistance | 5052, 5083, 5086 |
| 6xxx | Magnesium and silicon | Yes | Balanced strength, machinability, weldability and corrosion resistance; extrudes well | 6061, 6063, 6082 |
| 7xxx | Zinc | Yes | Highest strength, machines well, generally not arc welded, lower corrosion resistance | 7075, 7050 |
| 8xxx | Other (iron, lithium) | Varies | Specialty: foil, conductor and aerospace aluminum-lithium alloys | 8011, 8090 |
Temper designations
The temper follows the alloy number after a hyphen. It can change strength by a factor of two or more for the same alloy, so a callout without one is incomplete.
| Temper | Meaning | Example |
|---|---|---|
| F | As fabricated, no property guarantees | Cast or extruded stock before treatment |
| O | Annealed, softest and most formable | 5052-O, 6061-O |
| H1x | Strain hardened only; second digit is hardness (2 = quarter, 4 = half, 8 = full hard) | 1100-H14, 3003-H14 |
| H3x | Strain hardened and stabilized | 5052-H32 (quarter hard, stabilized) |
| H116 / H321 | Special marine tempers for 5xxx with controlled corrosion resistance | 5083-H116 |
| T3 | Solution heat treated, cold worked, naturally aged | 2024-T3 |
| T4 | Solution heat treated, naturally aged | 6061-T4 |
| T5 | Cooled from hot working (extrusion) and artificially aged | 6063-T5 |
| T6 | Solution heat treated and artificially aged | 6061-T6, 7075-T6 |
| T651 / T6511 | T6 plus stress relief by stretching (T6511 adds minor straightening, for extrusions) | 6061-T651 plate, 6061-T6511 bar |
| T73 / T7351 | Overaged for stress corrosion cracking resistance, at some loss of strength | 7075-T73 |
Typical strength of common alloys and tempers
| Alloy and temper | Yield, MPa (ksi) | Tensile, MPa (ksi) | Elongation | Density (g/cm³) |
|---|---|---|---|---|
| 1100-H14 | 117 (17) | 124 (18) | About 9% | 2.71 |
| 2024-T3 | 345 (50) | 483 (70) | About 18% | 2.78 |
| 3003-H14 | 145 (21) | 150 (22) | About 8% | 2.73 |
| 5052-H32 | 193 (28) | 228 (33) | About 12% | 2.68 |
| 5083-H116 | 228 (33) | 317 (46) | About 16% | 2.66 |
| 6061-T6 | 276 (40) | 310 (45) | About 12% | 2.70 |
| 6063-T5 | 145 (21) | 186 (27) | About 12% | 2.69 |
| 6063-T6 | 214 (31) | 241 (35) | About 12% | 2.69 |
| 7075-T6 | 503 (73) | 572 (83) | About 11% | 2.81 |
| Cast tooling plate (MIC-6 type) | About 105 (15) | About 166 (24) | About 3% | About 2.7 |
Typical values from published handbook data for thin sheet or small sections, not specification minimums. Minimums (for example ASTM B209) run lower and vary with thickness. Design to the minimum in the spec your drawing names.
Fabrication ratings and typical uses
| Alloy and temper | Machinability | Weldability (arc) | Formability | Anodize response | Typical uses |
|---|---|---|---|---|---|
| 1100-H14 | Poor (gummy) | Excellent | Excellent | Good, bright clear | Chemical equipment, reflectors, spun parts, trim |
| 2024-T3 | Good | Poor | Fair | Fair; copper gives a yellowish, less protective film | Aircraft structure and fittings, high-fatigue parts |
| 3003-H14 | Poor to fair | Excellent | Excellent | Good for protection, less even for cosmetics | HVAC, tanks, cookware, general sheet |
| 5052-H32 | Fair | Excellent | Very good | Good | Sheet metal enclosures, chassis, marine and fuel tanks |
| 5083-H116 | Fair | Excellent | Good | Good, protective | Boat hulls, marine plate, cryogenic and pressure vessels |
| 6061-T6 | Good | Good, with strength loss at weld | Fair in T6, good in O or T4 | Good | Machined parts, frames, fixtures, general structure |
| 6063-T5 / T6 | Fair (softer than 6061) | Good | Good | Excellent, most even cosmetic finish | Architectural extrusions, trim, frames, heat sinks |
| 7075-T6 | Excellent | Poor (not used for structural arc welds) | Poor in T6 | Good; hardcoat well | Aerospace and high-load machined parts, molds, sporting goods |
| Cast tooling plate (MIC-6 type) | Excellent, very stable | Fair, rarely welded | Not formed | Poor for cosmetics (mottled) | Fixture and jig plates, vacuum plates, inspection bases |
Ratings are relative and assume standard shop practice. Cast tooling plate is sold under several trade names; it is chosen for flatness and stability after machining rather than strength.
Quick picker by process
| If the part is mainly | Start with | Avoid |
|---|---|---|
| Bent sheet metal | 5052-H32 | 6061-T6 at tight radii, 7075-T6, 2024-T3 |
| CNC machined | 6061-T6, or 7075-T6 for strength | 1100, 3003, 5052 for detailed features |
| Welded | 5052, 5083, 6061 (sized for weld zone) | 7075, 2024 |
| Cosmetic anodized | 6061 or 6063, one alloy per assembly | 2024, cast plate, mixing alloys |
| Marine or salt exposure | 5052, 5083, 6061 | 2024, 7075 without a coating |
| Flat fixture plate | Cast tooling plate or 6061-T651 | Cold-worked sheet tempers that move when machined |
Values are typical published data for common product forms and are for comparison. A shop confirms machinability, bend radius and finish against its own equipment, and stock availability varies by alloy, temper and thickness.
Get a quote
Upload your file with the alloy and temper and get one matched quote from a partner shop, usually in about 24 hours.
- Free quote in about 24 hours
- No minimum order
- No account needed to start
STEP · STL · IGES · DWG · DXF · SLDPRT · and more
No CAD file? Describe your project instead
Frequently asked questions
What are the most common aluminum alloys for custom parts?
6061-T6 for machined and general structural parts, 5052-H32 for bent sheet metal, and 7075-T6 for high-strength machined parts. 6063 is common for extrusions and cosmetic anodized profiles.
What does the T6 in 6061-T6 mean?
T6 means the alloy was solution heat treated and then artificially aged to near peak strength. T651 adds stress relief by stretching, which is the usual temper for 6061 plate because it moves less when machined.
What does H32 mean in 5052-H32?
H3x tempers are strain hardened and stabilized, and the second digit 2 means quarter hard. 5052 is not strengthened by heat treatment, so cold work is how it gets its strength.
Which aluminum alloy is strongest?
Among common stocked alloys, 7075-T6 at about 503 MPa typical yield. Some 7xxx aerospace alloys such as 7050 and 7068 are similar or higher. 2024-T3 is next, then 6061-T6 at about 276 MPa.
Which aluminum alloys can be welded?
1100, 3003, 5052, 5083 and 6061 are routinely arc welded. Heat-treated alloys lose strength near the weld, so welded 6061 is sized for weld-zone strength. 2024 and 7075 are generally not arc welded for structural joints.
Sources
- Aluminum Association, Aluminum Standards and Data
- Aluminum Association, International Alloy Designations and Chemical Composition Limits (Teal Sheets)
- ANSI H35.1, Alloy and Temper Designation Systems for Aluminum
- ASTM B209, Aluminum and Aluminum-Alloy Sheet and Plate
- ASM Handbook, Volume 2 (ASM International)
- Arconic MIC-6 cast aluminum plate data sheet
- MatWeb material property data